Blowhead Reduces Container Defects

Johnson Radley Ltd has taken another step forward in developing the potential of its hot end handling material Cerberite for reducing ware damage during forming. Following on from the mould top plate launched last year to prevent checks in the area immediately below the finish, the company has turned its attention to the blowhead, which can cause checks and crizzles on the top of the finish closure.

Author
Un-named
Origin
Unknown
Journal Title
Glass 75 3 1998 84
Sector
Container glass
Class
C 1134