Blowhead Concept Continues To Streamline Production

Blowheads with an investment cast base of through-hardened stainless steel, combined with a proprietary HR Series alloy insert and designed to handle a range of sizes through the use of removable inserts instead of there being a single size for each blowhead, are referred to in this article. A number of advantages are claimed and described, not the least of these being better dimensional stability, leading to higher output.