Biomin Bioglass Toothpaste May Better Protect Sensitive Teeth And Find Its Way Into The Us Market

Queen Mary University London reports that scientists have developed a new and improved bioglass toothpaste formulation called BioMin. In addition to addressing tooth sensitivity, BioMin's makers say the toothpaste also can help prevent tooth decay and acid erosion, thanks to the ability of the bioglass to form a protective enamel-mimicking layer and slowly release fluoride into the mouth. BioMin is not just another version of bioglass, it has some important benefits over the original NovaMin formulation. To read the story in full, please visit: ceramics.org/ceramic-tech-today/biomaterials/biomin-bioglass-toothpaste-may-better-protect-sensitive-teeth-and-find-its-way-into-us-market

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 95 6 2016 22-23
Sector
Special Glass
Class
S 4274

Request article (free for British Glass members)

Biomin Bioglass Toothpaste May Better Protect Sensitive Teeth And Find Its Way Into The Us Market
Am Ceram Soc Bull 95 6 2016 22-23
S 4274
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
19 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.