Biomedical Thermodynamics And Implantology Aspects Of Biocompatible Glass-Ceramics And Otherwise Modified Inorganic Materials And Surfaces

Some historical and recent attitudes aimed to bioactive materials are reviewed. The theory of bridging and non-bridging oxygen is reconsidered as well as the acid and alkali treatment of titanium surface necessary to achieve a good osteointegration. Some theoretical models to characterise properties are also reviewed.

Author
J. Sestak Et Al
Origin
Institute Of Physics Of The Academy Of Sciences, Czech Republic
Journal Title
Advanced Materials Research Vols 39-40 (2008) 329-334
Sector
Glass Ceramics
Class
GC 708

Request article (free for British Glass members)

Biomedical Thermodynamics And Implantology Aspects Of Biocompatible Glass-Ceramics And Otherwise Modified Inorganic Materials And Surfaces
Advanced Materials Research Vols 39-40 (2008) 329-334
GC 708
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.