[Bioglass] An Update On Mo-Sci'S Novel Borate Glass Fibers

In 2011 USA-based Mo-Sci Corp leveraged researched conducted at the Missouri University of Science & Technology and developed a unique and perhaps revolutionary medical product. Dubbed "DermaFuse" this product is composed of a special formula of cottony borate glass nanofibres that appear to have a knack for healing deep, complicated and long-standing wounds. This article provides an update as to where the research has led today.