Biodegradable Shear Spray Lubricants

As the world gives more attention to the environment, biodegradable lubricants are becoming increasingly polular and interest in their properties is growing. This article discusses the subject of biodegradability and makes reference to the Biosol range of shear spray lubricants which have been in use for many years.