Bioactivity Characterization And A Full Factorial Design On The Adhesive Strength Of Air Plasma Sprayed Ha-Tio2 Coated Ti

Series of Atmospheric Plasma Spray Coatings were made on titanium substrates based on a Full Factorial Design. Three parameters (number of pass of the bond coat, amount of TiO2 into coating powder precursor and the spray distance) with three levels were selected to investigate their effects on the bonding strength and bioactivity. The coatings were characterised in terms of adhesion and bioactivity. Results indicated that all parameters had positive effect on the bonding strength of the coatings. R2 and R2 adjusted values were found to be 98.9% and 96.9% respectively, which proved the reliability of the regression and ANOVA analyses.

Author
Z Zumrut Et Al
Origin
Istanbul Technical University
Journal Title
J Aust Ceram Soc 49 2 2013 95-103
Sector
Special Glass
Class
S 4027

Request article (free for British Glass members)

Bioactivity Characterization And A Full Factorial Design On The Adhesive Strength Of Air Plasma Sprayed Ha-Tio2 Coated Ti
J Aust Ceram Soc 49 2 2013 95-103
S 4027
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.