Bioactive Ceramics For Skeletal Repair

One of the great challenges facing materials science and technology today is the development of a new generation of biomaterials to repair the body. Materials need to be designed to last longer and to aid the regeneration of tissues as opposed to replacing them.

Author
L H Hench
Origin
University Of London
Journal Title
Ceramic Technology International 1997 29-32