Biaxial Flexutre Strength And Dynamic Fatigue Of Soda-Lime-Silica Float Glass

The strength and dynamic fatigue behaviour of float glass was investigated using biaxial flexure tests. The samples were tested using the ring-on-ring (ROR) biaxial flexure test geometry, and the data analysed using a conventional two-parameter Weibull distribution.

Author
M H Krohn
Origin
Pennsylvania State University, Usa
Journal Title
J Am Ceram Soc 85 7 2002 1777-1782