The Bi203-Nb205-Nio Phase Diagram

The Bi2O3-Nb2O5-NiO phase diagram at 1100 deg C was determined by means of solid-state synthesis, X-ray diffraction, and scanning electron microscopy.

Author
M Valant & D Suvorov
Origin
Advances Materials Dept, Jamova, Slovenia
Journal Title
Jacs 88 9 2005 2540-2543