Benefits Of Nepheline Syenite In Technical Glass Melting

The effect of replacing calcined alumina with nepheline syenite in the melting of borosilicate and soda-lime potassium glass compositions is discussed.

Author
M Galewicz, W Hejnar
Origin
Krosno Glass Works, Poland
Journal Title
Glass 1992 69 2 71
Sector
Special Glass
Class
S 610

Request article (free for British Glass members)

Benefits Of Nepheline Syenite In Technical Glass Melting
Glass 1992 69 2 71
S 610