The Benefits Of Dry-Batch Optimisation In A Float Glass Plant

Nalco's Dry Batch Optimizer technology has been successfully used in the container glass industry to improve the operation of batch feed systems, reduce batch feed system maintenance and decrease batch moisture content without any effect on product quality. The technology was recently trialed at a US float glass plant and this article outlines the findings.