Benefits From Cts Technology

Swiss company Luscher AG's JetScreen Computer-to-Screen (CtS) technology is well known internationally for the digital production of large format screen printing stencils without the use of process film. The systems are suitable for all kinds of glass printing applications. The maximum screen frame size can be up to 4100mm x 9000mm, without fitting a strip or image holder. JetScreen with an equipped piezo print head with 256 nozzles produces excellent copying image resolution and reproduction. Artistic design and decoration or glass and technical printing of all types and sizes of plate glass, including three dimensional hollow glass forms, is achieved using the most cost efficient commercial silk screening procedure. For more information please see the website: www.luescher.com

Author
Un-named
Origin
Unknown
Journal Title
Glass International Nov/Dec 2005 28
Sector
Flat glass
Class
F 1941b

Request article (free for British Glass members)

Benefits From Cts Technology
Glass International Nov/Dec 2005 28
F 1941b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.