Batch/Cullet Preheater Experience At Ardagh Glass

In this article, the authors discuss experiences and measuring data for the application of a preheating system on an end port furnace at Ardagh in The Netherlands. Particular attention is paid to the effects of the preheating system on the energy consumption of the furnace and regenerator.