Batch Redox And Colour Control

The redox derived from batch materials including the contribution from cullet is discussed and some examples are given of the effect of furnace conditions and operating methods on glass colour.

Author
R D Wright
Origin
Rockware Group Plc
Journal Title
Glass Technology 1988 29 3 91-93
Sector
Container glass
Class
C 137