Batch To Oxide Percentage And Oxide Percentage To Batch Calculations For Glass Processing

Every glass product is prepared from a recipe made up of different raw materials. This paper describes a procedure which has been developed for the preparation of these recipes.

Author
D Oksoy And L D Pye
Origin
Alfred University, Usa
Journal Title
Glass Technology 33 4 August 1992 141-148