Batch Materials - Srco3 - Celestite

The celestite and strontium carbonate industries are intrinsically linked. Indeed, virtually the entire global output of celestite is utilised in the manufacture of the carbonate since SrCO3 rarely exists in nature. Celstite is the mineral source of strontium carbonate, produced either by the black ash route or by direct conversion with soda ash. For the former, the carbonate is formed via a dry or calcining method, whereby strontium sulphate is reduced by coal to form a water-soluble sulphide and is filtered to remove any large impurities. Then either soda ash or carbon dioxide is used to convert the sulphide to a precipitated carbonate.

Author
Un-named
Origin
Unknown
Journal Title
Asian Glass April/May 2002 44-45, 47
Sector
General
Class
G 2508

Request article (free for British Glass members)

Batch Materials - Srco3 - Celestite
Asian Glass April/May 2002 44-45, 47
G 2508
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.