[Batch] Does The Use Of Calcined Lime Help Solve The Batch Caking Problem?

Vidrala's glass technology manager, Dr Estela Alejandro, reports here on the experiments and subsequent industrial tests on the use of calcined lime to solve the batch caking problem.