Batch Charging - Enhancing Furnace Performance

In recent years, the efficiency of glass furnaces has dramatically improved. An area which has often been overlooked is the importance of a well-designed batch charging system in the overall performance and efficiency of the glass melting process. Controlling the distribution of batch across the melter can improve melting efficiency and increase furnace life.