Batch Chargers Influence Furnace Operation And Efficiency

In this paper the auther explains how the latest developments in batch charging systems and subsequent control of the glass level can assist the furnace manager and contribute significantly towards the production of the highest quality glass.

Author
H Drescher
Origin
Zippe, Germany
Journal Title
Glass Int 23 2 May-June 2000 9-10