Barium Gallosilicate Glasses. Part 1, Transformation Range Behaviour

The glass forming region of the barium gallosilicate ternary system has been determined and transformation range behaviour studied using transformation range viscosity, glass transformation temperature, and dilatometric softening point measurements.

Author
C M Shaw, J E Shelby
Origin
Nys College Of Ceramics At Alfred University
Journal Title
Phys Chem Glasses 1990 31 5 199-204