Back To The Days Of Mechanical Polishing Of Crystal Glassware

Mechanical glass polishing of crystal glassware was used for many years before the introduction of acid polishing. It was a multi-stage process; a sandstone wheel was used to decoratively cut the crystal ware. This left a coarse surface which was then smoothed using a segmented poplar wood wheel or a dense cork wheel. Pumice powder being applied by hand until the cut was brought up to a dull finish. Finally, it was polished using a felt or brush wheel and rouge (Fe203) which was applied by hand to give a brilliant polished finish on the cut faces.

Author
N B Kirk & D A Dalton
Origin
British Glass
Journal Title
Int Crystal Fed Tech Conf, Sweden 14/15 Sept 1995 178-185
Sector
Domestic glass
Class
D 246

Request article (free for British Glass members)

Back To The Days Of Mechanical Polishing Of Crystal Glassware
Int Crystal Fed Tech Conf, Sweden 14/15 Sept 1995 178-185
D 246
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.