Automotive Glass Decorating Products

The use of glass decorating products in the automotive industry began around 40 years ago with the introduction of silver pastes for screenprinting. In the 1970s, when silver metal-based screenprinting pastes were widely used to defog and/or defrost backlites, the decoration of automotive glass leaped forward when car makers introduced the technqiue of gluing glass into the car bodies, which required protection of the polyurethane glue. Glass enamels were the ideal solution. In this article the author looks at the history, current and future developments & requirements of the various product groups used to decorate automotive glass.

Author
N Westra
Origin
Johnson Matthey
Journal Title
Glass Worldwide Sept-Oct 2006 31-32, 34
Sector
Flat glass
Class
F 2093

Request article (free for British Glass members)

Automotive Glass Decorating Products
Glass Worldwide Sept-Oct 2006 31-32, 34
F 2093
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.