Automatic Handling Of Thin Sheet Glass

An experimental investigation into the frequency parameters and the oscillation character of a symmetrically vacuum-held sheet was carried out with dependence on the actual conditions of the handling cycle. The sheet dimensions, the material properties and the position of four gripping elements used for sheet handling were also taken into account.