An Automated Rotating Cylinder Viscometer For Glass

The automation of a rotating cylinder viscometer for specific glass applications is presented. Viscosity is a key parameter of glass manufacture and influences melting and forming processes. For high viscosities, a fibre elongation method is used while the rotating cylinder method is preferred for lower viscositites. This method was first used by Lillie and has become, over the years, a standard method for measuring viscosities of glasses at high temperature.

Author
D Germond & S Vignesoult
Origin
Saint-Gobain Recherche
Journal Title
Fundamentals Of The Glass Manufacturing Process 1991, Esg Conf. 15-17
Sector
General
Class
G 1033

Request article (free for British Glass members)

An Automated Rotating Cylinder Viscometer For Glass
Fundamentals Of The Glass Manufacturing Process 1991, Esg Conf. 15-17
G 1033
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.