Attack Of Fluorides In Silica And Glass

The discovery of the change of the optical activity of a mixture of tartaric acid and antimony fluoride (SbF3) during storage in a glass container was applied to a simple precise method of determining the resistance of silica and glasses to hydrofluoric acid.