Atomic Structure And Dissolution Properties Of Yttrium-Containing Phosphate Glass

A classical molecular dynamics simulations of three compositions of yttrium-containing phosphate glasses, to study the atomic structure around yttrium, and understand how yttrium incorporation will affect the glass dissolution rate, has been undertaken. The Y-O bond length is about 2.2A and the coordination number is 6.3. To avoid effects due to different network connectivities, compositions were chosen to keep the Qn distribution and network connectivity roughly consistent, which was confirmed through direct calculation.

Author
Y Fu, J K Christie
Origin
Loughborough University
Journal Title
Int J Appl Glass Sci 8 2017 412-417
Sector
Special Glass
Class
S 4479

Request article (free for British Glass members)

Atomic Structure And Dissolution Properties Of Yttrium-Containing Phosphate Glass
Int J Appl Glass Sci 8 2017 412-417
S 4479
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.