Atomic Environments In Binary Lead Silicate And Ternary Alkali Lead Silicate Glasses

High resolution x-ray photoelectron spectroscopy (HRXPS) has been used to obtain binding energy information for the Pb 4f, 4d and 5d, Si 2p, Na 1s, Li 1s and 01s photoelectron peaks, along with the O KLL Auger transitions and valence band spectra in glasses of a general formula xPb0(10x)Si02 (0

Author
I A Gee Et Al
Origin
University Of Warwick, Uk
Journal Title
Phys Chem Glasses 42 6 2001 339-348