Atmospheric Corrosion Of A New, Fast Glass Powder Sensor

The assessment of environmental conditions is necessary to prevent damage on art objects. One possibility would be to detect single parameters such as humidity or a certain pollutant. However, these measurements do not give information ont he actual impact of the environment on materials. As an alternative sensitive glasses can be exposed, which react faster than art objects and may thus act as an early warning system for corrosive effects. By evaluating the changes observed on the sensor glass, conclusions about the environmental conditions can be drawn.

Author
A Krickser Et Al
Origin
Bavarian Centre Appl Energy Research
Journal Title
Icg Extended Abstracts 2 2001 273-274
Sector
Special Glass
Class
S 2684

Request article (free for British Glass members)

Atmospheric Corrosion Of A New, Fast Glass Powder Sensor
Icg Extended Abstracts 2 2001 273-274
S 2684
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.