Assortment Production Solutions

Food and drink manufacturers increasingly need to create products that stand out on the shelves. As a result, packaging and containers are becoming increasingly complex. In this article the author highlights how assortment production can reduce the high number of job changes during the container manufacturing process.

Author
N Hargreaves
Origin
Bertram Elektronik, Germany
Journal Title
Glass International Dec-Jan 2014 42-43
Sector
Container glass
Class
C 5058