Assisting The Smooth Manufacture Of Square Bottles

This article describes how, when a bottle producer in Mexico was commissioned by one of its customers to make a square-shaped beverage bottle, Pyrotek technical staff and sales engineer, Fernando Jauregui helped design a stacker bar insert that would effectively handle the shape. Given the customer's requirements, Pyrotek's P-25W carbon-carbon inserts were crafted to fit the company's existing stacker bars. Made using a process where carbon is reinforced with carbon fibres, the inserts exhibit excellent strength, good wear resistance, low edge thermal conductivity and are engineered to last longer than other similar materials. For more information, please visit: www.pyrotek.info/glass

Author
Un-named
Origin
Unknown
Journal Title
www.Pyrotek.Info/Glass
Sector
Container glass
Class
C 5130

Request article (free for British Glass members)

Assisting The Smooth Manufacture Of Square Bottles
www.Pyrotek.Info/Glass
C 5130
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.