Asia-Pacific Region Delivers For Heye

Heye International has reported significant sales growth throughout the Asia-Pacific region. One of the international glass container industry's leading suppliers of high performance production technology and know-how, Heye has installed over 40 production lines throughout the region since 2012, having successfully completed projects in Australia, China, India the Philippines, S Korea, Taiwan, Thailand and Vietnam. Most of these installations now feature NNPB forming process technology.