Asahi-Schwebel To Launch Improved Glass Cloths For Pcbs

Japan's Asahi-Schwebel plans to introduce two types of high-value-added glass cloth in 2005 for use in printed circuit boards: One is AZ Cloth, made from non-twisted yarn & featuring highly uniform thickness; the other is ultra-thin glass cloth, 13 micrometers in thickness, for use in upgraded substrates. Japan's major producer of glass cloth is about to start sample consignments with the aim of drawing up a detailed production & sales schedule on the basis of customer response to the new products. It is expected that the existing production facility will be expanded to launch new production & that the first sales will be made in Japan & then overseas. AZ Cloth is composed of non-twisted yarn with a roughly square cross-section that contributes to the high regularity in the thickness of the cloth. By contrast, conventional cloths have irregular thickness.

Author
Un-named
Origin
Unknown
Journal Title
Glassonline News Release 29/07/04
Sector
News Items
Class
N 1545

Request article (free for British Glass members)

Asahi-Schwebel To Launch Improved Glass Cloths For Pcbs
Glassonline News Release 29/07/04
N 1545
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.