Application Of Urbain'S Model For Slag Systems In The Estimation Of Viscosity Of Some Commercial Glasses

For the estimation of viscosity of glasses and slags, several model equations are generally used, most of which involve three or more empirical constants. The most widely used model for slag systems, proposed by G Urbain, uses two constants, which are interrelated linearly. Urbain examined data for 54 oxides, silicates and alumino-silicates to establish his model. This paper establishes the validity of Urbain's model for a large number of glasses ranging from binaries, ternaires to more complex systems. The paper also examines the possibility of relating the empirical constants to optical basicity with the ultimate objective of estimation of glass viscosity solely from the composition and optical basiscity of the melt.

Author
S K Pal Et Al
Origin
Cgcri, India
Journal Title
Trans Ind Ceram Soc 62 4 2003 213-216
Sector
Special Glass
Class
S 2928

Request article (free for British Glass members)

Application Of Urbain'S Model For Slag Systems In The Estimation Of Viscosity Of Some Commercial Glasses
Trans Ind Ceram Soc 62 4 2003 213-216
S 2928
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.