Application Of Ultrasonic Measuring Techniques In Industrial Glass Melting

Potential applications of ultrasonic measurements in glass melts have been studied, using a system comprising ultrasonic waveguides of polycrystalline translucent alumina. Detection of bubbles in a feeder, measurement of glass flow velocities, glass temperature, and residual refractory wall thickness are among possible applications.