Application Of Thermometry To Analysis Of Glasses And Batch Materials.

After an introduction to the theoretical basis of thermometric analysis the apparatus and modifications made by the authors for their special problems are described. Results are given for the determination of boron in glasses and raw materials as well as in slags and compared with results obtained by classical methods.