The Application Of Radiation Modification Route For Chalcogenide Glasses

A post-technological modification route to optimise the optical properties of chalcogenide glasses owing to their treatment in the conditions of a high-energy stationary radiation field formed by 60COy-quanta is considered in this paper, with examples of stoichiometric AS2S3-GES2 and non-stoichiometric AS2S3-GE2S3 glasses. It was shown that both the energetic and geometric features of the glass-forming network should be taken into account to introduce numerical criterion for radiation modification efficiency.

Author
O Shpotyuk Et Al
Origin
Jan Dlugosz University, Poland
Journal Title
Gmpa 4/2005 90-92
Sector
Special Glass
Class
S 2994

Request article (free for British Glass members)

The Application Of Radiation Modification Route For Chalcogenide Glasses
Gmpa 4/2005 90-92
S 2994
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.