Application Of Particle Desorption Mass Spectrometry To Glass Surfaces

It has been demonstrated that Californium-252 PDMS can be used to determine differences in glass composition and the effects of chemical treatments on glass surfaces.

Author
M U D Beug-Deeb, E A Schweikert
Origin
Texas A&M University
Journal Title
Ceramic Bulletin 1987 66 11 1635-1639