Application Of Mossbauer Spectroscopy To Iron Ions In The Lithium Tellurite Glasses

The local structure around iron atoms in four series of lithium tellurite glasses is studied by means of Mossbauer spectroscopy with 57 Co(Pd) and Fe foil as the gamma-ray source and reference.