The Application Of The Flame Photometer And The Spectrograph To The Analysis Of A Soda-Lime Glass

The determination of alkalis and calcium in glass by flame photometry and of calcium, aluminium, and magnesium by spectrography has been investigated. Two flame photometers were used: an Evans Elecroselenium LTD filter photometer and a flame spectrometer.