Application Of Diret Emission X-Ray Analysis To Control And Research In The Glass Industry

X-ray fluorescence and direct emission spectroscopy are discussed as analytical tools for quality control in the glass industry. The main applications are the quantitative analysis of light elements in glass, determinations made on low concentrations and analysis of distribution of elements in a specimen with particular regard to comparison with the various quantitative measurements available for determining heterogeneity in glasses.

Author
J Duchateau
Origin
Unknown
Journal Title
Vii International Congress On Glass Brussels Paper 88 1965
Sector
Primary Papers
Class
PP 1342

Request article (free for British Glass members)

Application Of Diret Emission X-Ray Analysis To Control And Research In The Glass Industry
Vii International Congress On Glass Brussels Paper 88 1965
PP 1342
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.