Anticorrosion Glass-Enamel Coatings

Corrosion-resistant, fluorine-free coatings based on carbonate ores containing small amounts of manganese have been developed.

Author
A V Sarukhanishvili Et Al
Origin
Georgian V I Lenin Polytechnical Inst, Sci-Res Inst Enamels Chem Mach
Journal Title
Glass And Ceramics 1987 44 7-8 323-325