Anomalies Of Thermoelastic Properties In Fine-Grained Glass-Ceramics

The results of measurements of acoustic characteristics (velocities, V, and temperature coefficients of velocities, TCV, for ultrasonic waves with different polarizations) are presented for glasses and glass-ceramics in the lithium aluminosilicate system.