Annealing Process For Glass Products And Their Final Inspection

The author describes briefly the method elaborated and applied at the state glass research institute at Hradec Kralov.

Author
V Novotny
Origin
Czech
Journal Title
Sklar Keram., 35 4 1985 106-11
Sector
Primary Papers
Class
PP 1493

Request article (free for British Glass members)

Annealing Process For Glass Products And Their Final Inspection
Sklar Keram., 35 4 1985 106-11
PP 1493