The Annealing Of Cellular Glass

In this article the author discusses the annealing of cellular glass, a process which is integral to the design and operation of a foamed glass plant.

Author
H Strauven
Origin
Glapor Werk, Germany
Journal Title
Glass International Dec-Jan 2016 49-50
Sector
Glass Fibre
Class
GF 720

Request article (free for British Glass members)

The Annealing Of Cellular Glass
Glass International Dec-Jan 2016 49-50
GF 720