Ancient Glass In Southern Turkey

Investigations of glass vessels n the bolge museum in Adana (Turkey) and of Canadian excavations at Anemurium (Turkey) are reported.

Author
Em Stern
Origin
Unknown
Journal Title
Glastechnische Berichte 57 5 1984 132-139