Analytical Models For High-Temperature Corrosion Of Silica Refractories In Glass-Melting Furnaces

Corrosion of refractory silica brick used to line the crown of many glass-melting furnaces is a serious problem in furnaces using oxygen-fuel rather than air-fuel mixtures. To better understand and to quantify this process, analytical models are utilised to evaluate the importance of four potential rate-limiting processes: a) gas-phase transport of NaOH to the crown surface; b) diffusion of sodium-containing reactants through a liquid product layer that forms on the brick face; c) gas-phase discussion of NaOH into refractory pores; and d) chemical-kinetic limitations at the silica grain surface. Predictions are compared with reported corrosion rates and product compositions previously determined by post-mortem analysis of refractory samples.

Author
R H Nilson Et Al
Origin
Sandia Nat Labs, Usa
Journal Title
Glass Sci Technol 76 3 2003 136-151
Sector
Refractories
Class
R 537

Request article (free for British Glass members)

Analytical Models For High-Temperature Corrosion Of Silica Refractories In Glass-Melting Furnaces
Glass Sci Technol 76 3 2003 136-151
R 537
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.