Analytical Determination Of Impurities In Glassmaking Sands Containing At Least 95% Sio2

A method is described for the determination of low impurity levels such as Na, K, Mg, Ca, Al, Fe, Cr and Ti in glassmaking sands. The recommended procedures give a satisfactory reproducibility for the given elements. Although the TC concluded that the sand used did not seem to be homogeneous engough to serve as a real "reference material", it nevertheless presents analysts with a good opportunity to check their own practice in the determination of these elements.

Author
Un-named
Origin
A Peters
Journal Title
Glass Technology 34 6 1993 239-248
Sector
General
Class
G 1028

Request article (free for British Glass members)

Analytical Determination Of Impurities In Glassmaking Sands Containing At Least 95% Sio2
Glass Technology 34 6 1993 239-248
G 1028
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.