[Analysis - Wine Packaging] Wine Or Whine?

Asia's wineries remain loyal to glass for now, but emerging threats may change the landscape. In this article, Asian Glass looks at how SE Asia is fighting against the PET threat, whilst on the contrary China offers hope of a glass-filled future.