Analysis Of Various Plunger Materials Used In The Container Glass Industry

The achievement of high impact strength has a basic influence on the further development of lightweight container glass. Eleven non-returnable flint glass water bottles, produced by the NNPB process were tested for impact strength by repeated hitting on the upper contact area on the shoulder. Four different plunger materials were tested in a 12-section AIS Emhart machine. The test run was structured in an experimental and ananalytical part. The paper includes graphic and diagrammatic interpretations concerning impact strength, the elements from the plunger materials contained in the glass and furthermore, the change in the chemical composition of the plunger material after use. The aim of this analysis was to find an ideal plunger material, which satisfies the requirements of higher strength for lightweight glass containers.

Author
S Tanhofner
Origin
Gerhard-Mercator-Universitat-Gh, Germany
Journal Title
Glastech Ber Glass Sci Technol 72 11 1999 335-340
Sector
Container glass
Class
C 1479

Request article (free for British Glass members)

Analysis Of Various Plunger Materials Used In The Container Glass Industry
Glastech Ber Glass Sci Technol 72 11 1999 335-340
C 1479
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.